What it is
A new timber floor with a dip, showing a gap under a straight edge.
Why it matters
Out-of-flat floors look wavy, can squeak and affect how furniture sits.
How we check it
We put a straight edge and level on floors and measure any gap.
The fix
Rectify the subfloor and floor so it's within tolerance.
How common it is
We measure floors at handover, not just look at them.
What this means for your home
A timber or engineered floor that is not laid flat — humps, dips or lipping between boards — is both a trip and a wear problem, and it rarely improves with time. The flooring manufacturer's tolerances and the QBCC guide set how flat the substrate and the finished floor must be. A floor laid over an uneven substrate or without acclimatising the boards telegraphs every high spot, and the lipping catches feet and furniture. Caught at handover the floor layer is still contracted and the affected area can be re-laid or the substrate corrected. Afterwards it is a full-room removal to fix. We run a straightedge across the floors, check for movement and lipping at the board edges, and photograph the areas outside tolerance so they are made good before you are living with a floor that never sat right. We run a straightedge and photograph any lipping or dip against the flooring tolerance so the floor layer addresses it. A floor that was never laid flat does not improve — it wears unevenly and trips you at the same spot for years. Catching it at handover, while the installer is still contracted, is the difference between a localised re-lay and living with a floor that never sat right.
The standard
QBCC Standards and Tolerances Guide 2023, 15.8